Preventing Osmotic Coating Failure on Coastal Process Piping via Bresle Salt & Profile Control
CASE STUDY • MARINE & OFFSHORE

Preventing Osmotic Coating Failure on Coastal Process Piping via Bresle Salt & Profile Control

Coastal surface preparation audit, soluble chloride testing, fresh-water desalination washing, Sa 2.5 blasting, and high-build marine epoxy-polyurethane coating QC.

1. Asset Context

Asset: Exposed Carbon Steel Jetty & Manifold Piping · Sector: Marine & Offshore · Location: Nigerian Coastal Terminal Facility (Marine & Coastal Export Terminal — Anonymized)

2. Technical Challenge

Previous atmospheric maintenance coatings on jetty-adjacent piping blistered prematurely within months of application despite meeting target Dry Film Thickness.

3. Scope & Technical Approach

Conducted baseline Bresle patch soluble-salt extractions showing high marine chloride contamination embedded in shallow corrosion pits. Instituted high-pressure fresh-water washing prior to and between sweep blasting until conductivity limits complied with spec, combined with strict stripe coating and >= 3°C dew-point holds.

4. Execution Constraints

Constant sea spray, tidal mist fluctuations, and narrow dry-weather blasting windows.

5. Verified Findings & Client Operational Value

  • Identified and eliminated hidden ionic salt contamination before primer application.
  • Verified consistent Sa 2.5 cleanliness, compliant anchor profile, and statistical DFT across repaired manifolds.
  • Established repeatable coastal coating inspection hold points for terminal maintenance contracts.
6. Lessons & Engineering Considerations

Visual blast cleanliness (Sa 2.5) alone cannot reveal dissolved marine salts—quantitative Bresle salt testing is essential in coastal and offshore zones.

TECHNICAL & COMMERCIAL ENQUIRIES

Need Inspection or QA/QC Support?

Share your asset details, applicable engineering codes, and target project window with our technical team to initiate a quotation review.